dc.description.abstractIn a typical forming limit curve (FLC), the minimum major strain where the minor value is equal to zero is located at y axes. In many forming processes, failure occurs at this region. Many studies in literature indicates that minimum major strain value is obtained about at y axis. In this study, the minimum major strain value is not determined on the y axes and it was found to be offsetted from the y axes to the right about 0.04 strain for AA 2024-T4. This value could be important for evaluations of sheet metal forming processes. In this study, the reasons for the minimum major strain of setting of the forming limit curve for AA 2024-T4 were investigated. It was found that drawbead and heat treatment were most effective parameters for this offsetting. It is observed that offsetting result from pre-strain which occur for conducted tests with using draw-bead and residual stress arising from T4 heat treatment.en_US
dc.identifier.endpage536en_US
dc.identifier.issn1300-1884
dc.identifier.issn1304-4915
dc.identifier.issue3en_US
dc.identifier.scopusqualityQ2en_US
dc.identifier.startpage527en_US
dc.identifier.urihttps://hdl.handle.net/20.500.12452/17702
dc.identifier.volume29en_US
dc.identifier.wosWOS:000343887100010en_US
dc.identifier.wosqualityQ4en_US
dc.indekslendigikaynakWeb of Scienceen_US
dc.language.isotren_US
dc.publisherGazi Univ, Fac Engineering Architectureen_US
dc.relation.ispartofJournal Of The Faculty Of Engineering And Architecture Of Gazi Universityen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectNakajima Testen_US
dc.subjectForming Limit Curve (Flc)en_US
dc.subjectMinimum Major Strainen_US
dc.subjectAa2024-T4en_US
dc.titleINVESTIGATION INTO REASONS FOR MINIMUM MAJOR STRAIN OFFSETTING OF FORMING LIMIT CURVE OBTAINED WITH NAKAJIMA TEST FOR AA 2024-T4en_US
dc.typeArticleen_US

Dosyalar